16MnCr5 / 1.7131 - SteelNumber - Chemical composition, …
Properties of steel 16MnCr5 (1.7131) Weldability: It is a MnCr alloy steel, easily hot machinable and weldable Hardenability: It has a low hardenability and therefore it can show good core …
EN 1.7131 Steel 16MnCr5 Material Equivalent, Composition, Properties
16MnCr5 steel is generally used after carburizing and quenching, and is mainly used for manufacturing gears, worms, sealing bushings and other components. The following tables …
16MnCr5 Steel, Datasheet, Properties, Cross-Reference Table, …
16MnCr5 Carbon Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
16MnCr5 - Ovako
16MnCr5 is an alloyed case hardening steel used for e.g. mechanical engineering components.The steel can be M-treated in order to optimize the machinability. For additional …
This page is mainly introduced the 16MnCr5 Datasheet, including chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, …
16MnCr5 (UNI ) - Worldwide equivalent grades - Steel Number
European equivalent grade for Alloy special steel 16MnCr5 (UNI ): 16MnCrS5 (1.7139) Cross reference table for Steel 16MnCr5 (UNI ) and its European equivalent 16MnCr5 (1.7131) ( EN )
5115 Case Hardening Steel - 1.7131 - 16MnCr5 - SAE 5115
5115, also known as 16MnCr5 or EC80, is a cold work case hardening steel with a high surface hardness, a tough core and higher sulfur for better machining. 5115 case hardening steel finds …
Steel 16MnCr5: characteristics, properties, analogues - Metinvest
Steel grade 16MnCr5 is used for surface hardening when grouting, nitrocarburising, nitriding and for other types of surface chemical-thermal treatment. It is used to make shafts, axles, gears, …
Use only as reference size mm Testing at room temperature. Mod. of Elasticity long. Mod. of Elasticity tang. Specific Electric Resist. The symbol indicates temperature between 20 °C and …
16MnCr5 | 1.7131 - learn more - Materials Processing Europe
The steel grade 16MnCr5 is a case hardening steel with a carbon content between 0.14 and 0.19 %. It is intended for case hardening. In this process, carbon is introduced into the surface layer …